METHOD OF MAKING ANTIFRICTION PRODUCTS ABSTRACT OF THE DISCLOSURE In accordance with the proposed method of making anti- friction products, a porous carbon blank is heated up to 1,800 to 2,200°C and impregnated with molten silicon. The impregnation starts at a temperature of 2,100 to 2,200°C for 3 to 5 minutes, then at 1,800 to 2,050°C for 30 to 40 minutes. Thereafter, the blank is cooled down to a tempe- rature of 900 to 800°C at a rate of 30 to 40°C/min, then down to 200 to 150°C at a rate of 50 to 100°C/min. This permits obtaining products with an even phase distribu- tion, whereby their wear resistance and strength are im- proved.

308794

LandOfFree

Say what you really think

Search LandOfFree.com for Canadian inventors and patents. Rate them and share your experience with other people.

Rating

Method of making antifriction products does not yet have a rating. At this time, there are no reviews or comments for this patent.

If you have personal experience with Method of making antifriction products, we encourage you to share that experience with our LandOfFree.com community. Your opinion is very important and Method of making antifriction products will most certainly appreciate the feedback.

Rate now

     

Profile ID: LFCA-PAI-O-280050

  Search
All data on this website is collected from public sources. Our data reflects the most accurate information available at the time of publication.