Method of making high-strength, high-toughness steel with...

C - Chemistry – Metallurgy – 21 – D

Patent

Rate now

  [ 0.00 ] – not rated yet Voters 0   Comments 0

Details

148/31

C21D 8/00 (2006.01)

Patent

CA 1170151

ABSTRACT OF THE DISCLOSURE A high-strength, high-toughness steel with good work- ability is produced by working a steel containing 0.005-0.3% C and 0.3-2.5% Mn and optionally up to 1.5% Si, in the course of hot working thereof, at temperatures within the range of from the Ar3 point to 930°C or to 980°C (for a steel containing Nb, V, Ti and/or Zr) at an area reduction rate of at least 30%, and, in the course of cooling, rapidly cooling the steel in the ferrite phase precipitation temperature range when the ferrite phase has occu- pied 5-65% or 5.60% (for a steel with Si and/or Nb, V, Ti and/or Zr) of the steel, whereby a two-phase structure comprising ferrite and martensite is produced.

373816

LandOfFree

Say what you really think

Search LandOfFree.com for Canadian inventors and patents. Rate them and share your experience with other people.

Rating

Method of making high-strength, high-toughness steel with... does not yet have a rating. At this time, there are no reviews or comments for this patent.

If you have personal experience with Method of making high-strength, high-toughness steel with..., we encourage you to share that experience with our LandOfFree.com community. Your opinion is very important and Method of making high-strength, high-toughness steel with... will most certainly appreciate the feedback.

Rate now

     

Profile ID: LFCA-PAI-O-1291754

  Search
All data on this website is collected from public sources. Our data reflects the most accurate information available at the time of publication.