Abstract of the Disclosure Iron oxide particles are made by spray calcination and the oxide is reduced at least substantially in CO at temperatures between 800° and 1000° C The oxide is heat-treated prior to calcination or Cao is added to enhance formation of iron fibers. The reducing atmosphere may in parts include hydrogren or the last phase of reduction is carried out in hydrogen. The iron cake is cooled and broken up in a grinder. The resulting powder has low bulk density due to a fiber-like, nonporous consistency of its particles. Grinding may continue to increase bulk density.
234948
Dautzenberg Norbert
de Haas Hans
Grebe Klaus
Hewing Josef
LandOfFree
Method of making iron powder does not yet have a rating. At this time, there are no reviews or comments for this patent.
If you have personal experience with Method of making iron powder, we encourage you to share that experience with our LandOfFree.com community. Your opinion is very important and Method of making iron powder will most certainly appreciate the feedback.
Profile ID: LFCA-PAI-O-638432