Method of making rare-earth element containing permanent...

H - Electricity – 01 – F

Patent

Rate now

  [ 0.00 ] – not rated yet Voters 0   Comments 0

Details

75/148, 148/5

H01F 1/053 (2006.01) B22F 9/08 (2006.01) C22C 33/02 (2006.01) C22C 38/00 (2006.01) H01F 41/02 (2006.01)

Patent

CA 1276486

ABSTRACT OF THE DISCLOSURE A method for making rare earth-permanent magnets wherein a molten mass of a rare earth magnet alloy is produced such as by induction melting and while in a protective atmosphere is introduced in the form of a stream into a chamber having a protective atmosphere and a bottom portion containing a cooling medium, such as a cryogenic liquid which may be liquid argon. After cooling and solidification, the alloy is collected from the chamber and comminuted to produce particles. The particles are formed into a magnet body. Alternately, the stream may be atomized, as by striking the same with a jet of inert gas, to produce discrete droplets, which droplets are directed to the cooling medium at the chamber bottom for cooling, solidification and collection. *******

489948

LandOfFree

Say what you really think

Search LandOfFree.com for Canadian inventors and patents. Rate them and share your experience with other people.

Rating

Method of making rare-earth element containing permanent... does not yet have a rating. At this time, there are no reviews or comments for this patent.

If you have personal experience with Method of making rare-earth element containing permanent..., we encourage you to share that experience with our LandOfFree.com community. Your opinion is very important and Method of making rare-earth element containing permanent... will most certainly appreciate the feedback.

Rate now

     

Profile ID: LFCA-PAI-O-1322328

  Search
All data on this website is collected from public sources. Our data reflects the most accurate information available at the time of publication.