Method of manufacturing a modified polyhydroxy compound

C - Chemistry – Metallurgy – 07 – C

Patent

Rate now

  [ 0.00 ] – not rated yet Voters 0   Comments 0

Details

260/233, 403/26,

C07C 31/18 (2006.01) C07C 43/11 (2006.01) C08G 18/24 (2006.01) C08G 18/38 (2006.01) C08G 18/42 (2006.01) C08G 18/46 (2006.01) C08G 18/48 (2006.01) C08G 18/50 (2006.01)

Patent

CA 1306470

Abstract of the Disclosure A method of manufacturing a modified polyhydroxy compound, which is characterized in that a polyhydroxy compound is heated for 30 minutes or more at a tempera- ture ranging from 150 to 250°C under stirring and in the presence of tin, tin compounds such as tin halogenide, tin hydroxide and tin oxide. The polyhydroxy compound modified by this method is effective in improving the foamability and mechanical strength of urethane foam, when it is used as a raw material in the manufacture of urethane foam.

489110

LandOfFree

Say what you really think

Search LandOfFree.com for Canadian inventors and patents. Rate them and share your experience with other people.

Rating

Method of manufacturing a modified polyhydroxy compound does not yet have a rating. At this time, there are no reviews or comments for this patent.

If you have personal experience with Method of manufacturing a modified polyhydroxy compound, we encourage you to share that experience with our LandOfFree.com community. Your opinion is very important and Method of manufacturing a modified polyhydroxy compound will most certainly appreciate the feedback.

Rate now

     

Profile ID: LFCA-PAI-O-1176295

  Search
All data on this website is collected from public sources. Our data reflects the most accurate information available at the time of publication.