Method of manufacturing a pipeline pig having a rough...

B - Operations – Transporting – 29 – C

Patent

Rate now

  [ 0.00 ] – not rated yet Voters 0   Comments 0

Details

18/660

B29C 45/73 (2006.01) B08B 9/04 (2006.01) B29C 44/00 (2006.01) B29C 33/02 (2006.01)

Patent

CA 1304205

65224-373 Abstract of the Invention A method of making a foam pig having a highly textured and tough surface for use in cleaning the interior wall of a pipe line, the pig being formed by heating a metallic mold which defines the exterior configuration of the pig, injecting urethane base foam mixture into the heated mold, and curing the injected urethane foam before removing the cured pig from the mold. The mold should be heated to a temperature sufficient to produce a tough surface texture on the completed pig defined by closely spaced indentations of about one-half to three millimeters in depth, the indentations being formed by bubbles in the urethane foam base mixture on the surface of the mold.

563602

LandOfFree

Say what you really think

Search LandOfFree.com for Canadian inventors and patents. Rate them and share your experience with other people.

Rating

Method of manufacturing a pipeline pig having a rough... does not yet have a rating. At this time, there are no reviews or comments for this patent.

If you have personal experience with Method of manufacturing a pipeline pig having a rough..., we encourage you to share that experience with our LandOfFree.com community. Your opinion is very important and Method of manufacturing a pipeline pig having a rough... will most certainly appreciate the feedback.

Rate now

     

Profile ID: LFCA-PAI-O-1232629

  Search
All data on this website is collected from public sources. Our data reflects the most accurate information available at the time of publication.