METHOD OF PREPARING "-Al2O3 Abstract of the Disclosure .beta."-Al2O3 is a highly desirable material for serving the double function of solid electrolyte and separator in a re- chargeable battery that employs sodium, Na, as the anode and sulfur, S, as the cathode. But conventional means for manufacturing the .beta."-Al2O3 require temperatures between 1400 and 1600°C. By reacting .theta.-Al2O3 with Na2O, or a compound that yields Na2O on decomposition, the desired .beta."-Al2O3 is obtained at temperatures as low as 950°C.

271787

LandOfFree

Say what you really think

Search LandOfFree.com for Canadian inventors and patents. Rate them and share your experience with other people.

Rating

Method of preparing .beta."-a1.sub.2o.sub.3 does not yet have a rating. At this time, there are no reviews or comments for this patent.

If you have personal experience with Method of preparing .beta."-a1.sub.2o.sub.3, we encourage you to share that experience with our LandOfFree.com community. Your opinion is very important and Method of preparing .beta."-a1.sub.2o.sub.3 will most certainly appreciate the feedback.

Rate now

     

Profile ID: LFCA-PAI-O-935353

  Search
All data on this website is collected from public sources. Our data reflects the most accurate information available at the time of publication.