CA 1045370
METHOD OF PREPARING FERROELECTRIC CERAMICS ABSTRACT OF THE DISCLOSURE A process for preparing strengthened ferroelectric ceramics, which comprises sintering ceramic materials and then heat treating the sintered ceramics at a temperature from about 100°C to about 400°C lower than the final sintering temperature of ceramics, for about 1 to about 60 hrs., and then cooling at a rate from about 300°C to about 10°C per hour. Strengthened ferroelectric ceramics are obtained among the following ferro- electric ceramic compositions: I) Pb([B1]ATa1-A)O3-pbTiO3-pbZrO3, where [B1] is Mg, Zn, Cd, Sn, Mn, Fe, Co, and Ni when A=1/3 and [B1] is Li and Cu when A=1/4, II) Pb([B2]BTa1-B)O3-Pb([B3]CTa1-C)O3-PbTiO3-PbZrO3, where [B2] and [B3], [B2]?[B3], are Mg, Zn, Cd, Sn, Mn, Fe, Co and Ni when B and C=1/3, and [B2] and [B3], [B2]?[B3], are Li and Cu when B and C=1/4, III) Pb([B1]ATa1-A)O3PbTiO3-PbZrO3 with MnO2, where [B1] is Mg, Zn, Cd, Sn, Fe, Co and Ni when A=1/3, and [B1] is Li and Cu when A=1/4, and IV) Pb([B2]BTa1-B)O3-Pb([B3]CTa1-C)O3-PbTiO3-PbZrO3 with MnO2, where [B2] and [B3], [B2]?[B3], are Mg, Zn, Cd, Sn, Fe, Co and Ni when B and C=1/3, and [B2] and [B3], [B2]?[B3], are Li and Cu when B and C = 1/4.
219334
Nishida Masamitsu
Numata Kazunori
Ouchi Hiromu
LandOfFree
Method of preparing ferroelectric ceramics does not yet have a rating. At this time, there are no reviews or comments for this patent.
If you have personal experience with Method of preparing ferroelectric ceramics, we encourage you to share that experience with our LandOfFree.com community. Your opinion is very important and Method of preparing ferroelectric ceramics will most certainly appreciate the feedback.
Profile ID: LFCA-PAI-O-669329