ABSTRACT: Method of preparing a luminescent alkaline earth metal fluoroilalide activated by Eu2+ defined by the formula Me1-pEupFX (Me = Ba, Sr; X = Cl, Br, I; 0.001 ? p ? 0.20). MeF2 is suspended in water after which 1 mole of MeX2 per mole of MeF2 is dissolved in the suspension. The suspension, which may already contain europium, is evaporated to dryness at 50°C to 250°C. The obtained product is mixed with the additional re- quired amount of europium in the form of a europium halide and then is subjected to at least one temperature treatment at 600°C to 1000°C in a weakly reducing atmos- phere. The obtained reaction product is subjected, pos- sibly after being ground, to a final heating at 600°C to 850°C in an inert or weakly reducing atmosphere. - 15 -
236769
de Pauw Agnes D.m.s.
Pingault Francois
Stevels Albert L.n.
N.v. Philips Gloeilampenfabrieken
Na
LandOfFree
Method of producing a luminescent alkaline earth metal... does not yet have a rating. At this time, there are no reviews or comments for this patent.
If you have personal experience with Method of producing a luminescent alkaline earth metal..., we encourage you to share that experience with our LandOfFree.com community. Your opinion is very important and Method of producing a luminescent alkaline earth metal... will most certainly appreciate the feedback.
Profile ID: LFCA-PAI-O-10610