ABSTRACT OF THE DISCLOSURE Ethylenimine or oligomers thereof are polymerized in the presence of various cationic catalysts (taken in an amount of from 0.1 to 1.0 mol.% per each elementary unit) in mass at a temperature of from 40° to 55°C till about 10-25% conversion ratio of the ethylenimine cycles is reached, thereafter the polymerization process is inhibited with an alkali, the unused monomer (or oligomer) is distilled off, water is added in an amount of from 0.3 to 3.5 parts per each part of the oligomeric residue, and the polymerization process is completed at a temperature of from 5° to 25°C. The precipitate of the linear polyethylenimine crystallohydrate is separated, washed with water and dehydrated by way of drying in vacuum at a temperature within the range of from 40° to 100°C.

230671

LandOfFree

Say what you really think

Search LandOfFree.com for Canadian inventors and patents. Rate them and share your experience with other people.

Rating

Method of producing linear plyethylenimine does not yet have a rating. At this time, there are no reviews or comments for this patent.

If you have personal experience with Method of producing linear plyethylenimine, we encourage you to share that experience with our LandOfFree.com community. Your opinion is very important and Method of producing linear plyethylenimine will most certainly appreciate the feedback.

Rate now

     

Profile ID: LFCA-PAI-O-454072

  Search
All data on this website is collected from public sources. Our data reflects the most accurate information available at the time of publication.