ABSTRACT OF THE DISCLOSURE In bottom blown processes for the production of low carbon steels (i.e. less than 0.2% C), inert gas flushing employed at an intermediate point of the blow, provides more rapid and more efficient removal of N2. Thus, inert gas flushing is initiated at a point when the carbon content of the melt is in excess of 0.3%, and preferably in excess of 0.5%. When N2 is removed to a desired extent, full scale oxygen blowing is resumed to achieve the final degree of decarburization.
234487
LandOfFree
Method of producing low nitrogen steel does not yet have a rating. At this time, there are no reviews or comments for this patent.
If you have personal experience with Method of producing low nitrogen steel, we encourage you to share that experience with our LandOfFree.com community. Your opinion is very important and Method of producing low nitrogen steel will most certainly appreciate the feedback.
Profile ID: LFCA-PAI-O-430139