ABSTRACT A steel section 6 to 40 mm thick, emerging from a hot rolling mill at 1000 to 800°C is surface quenched for 2 to 6 seconds at a cooling rate of the order of 1.5 to 5 MW(megawatts)/m2. During subsequent self-tempering of the quenched surface by heat from the remainder, the section tends to an equalization temperature of 500 to 700°C.

303251

LandOfFree

Say what you really think

Search LandOfFree.com for Canadian inventors and patents. Rate them and share your experience with other people.

Rating

Method of producing steel sections of improved quality does not yet have a rating. At this time, there are no reviews or comments for this patent.

If you have personal experience with Method of producing steel sections of improved quality, we encourage you to share that experience with our LandOfFree.com community. Your opinion is very important and Method of producing steel sections of improved quality will most certainly appreciate the feedback.

Rate now

     

Profile ID: LFCA-PAI-O-743964

  Search
All data on this website is collected from public sources. Our data reflects the most accurate information available at the time of publication.