C22B 30/02 (2006.01) C22B 15/00 (2006.01) C22B 30/00 (2006.01) C22B 30/06 (2006.01) C25C 1/12 (2006.01) C25C 1/22 (2006.01)
Patent
CA 2167026
A method of recovering antimony and bismuth from copper electrolyte comprises the steps of immersing a pure copper material in the copper electrolyte, so that the iron ions are reduced from Fe3+ ions to Fe2+ ions, using a mixture of dilute sulfuric acid and sodium chloride adjusting the acidity or acidic concentration, to selectively elute the bismuth and antimony wherein if the final concentration of bismuth is adjusted to be 0.02 g/l or less in the bismuth election, it is possible to keep the maximum concentration of bismuth in the antimony eluate in the elution of antimony after selective bismuth elution to 0.01 g/l or less.
Ando Kouji
Fukui Atsushi
Tsuchida Naoyuki
Smart & Biggar
Sumitomo Metal Mining Co. Ltd.
LandOfFree
Method of recovering antimony and bismuth from copper... does not yet have a rating. At this time, there are no reviews or comments for this patent.
If you have personal experience with Method of recovering antimony and bismuth from copper..., we encourage you to share that experience with our LandOfFree.com community. Your opinion is very important and Method of recovering antimony and bismuth from copper... will most certainly appreciate the feedback.
Profile ID: LFCA-PAI-O-1826762