ABSTRACT OF THE DISCLOSURE A method of repairing damages in a superalloy component is disclosed wherein existing brazed joints and protective coatings are not harmed. The method entails the use of a silicon-free metal mixture comprising (i) a low melting alloy having a liquidus below the temperature to be used to deposit the metal mixture, (ii) an alloy melting above about 2100°F, and (iii) optionally nickel. The resultant repair has a solidus temperature of at least 1950°F, preferably at least 2000°.
589350
Iovene Michael A.
Lee Jack W.
Miller Jule A.
Avco Corporation
Sim & Mcburney
LandOfFree
Method of repairing damages in superalloys does not yet have a rating. At this time, there are no reviews or comments for this patent.
If you have personal experience with Method of repairing damages in superalloys, we encourage you to share that experience with our LandOfFree.com community. Your opinion is very important and Method of repairing damages in superalloys will most certainly appreciate the feedback.
Profile ID: LFCA-PAI-O-1228352