CA 2049276
A method of increasing the extraction of tellurium from copper electrorefining slime comprises leaching the slime with dilute sulphuric acid in a reactor under a partial oxygen pressure of up to 150 psi and at an elevated temperature between about 100 and 200°C until copper, nickel and substantially all of the tellurium is dissolved, thereby forming a leach slurry, and contacting the slurry with an appropriate reducing agent immediately after the leaching operation has been halted and the leaching reactor brough back to atmospheric pressure to reprecipitate any excessive quantities of silver and selenium solubilized during the leaching operation.
Claessens Pierre L.
White Carl W.
Nadeau Francois
Noranda Inc.
LandOfFree
Method of tellurium separation from copper electrorefining... does not yet have a rating. At this time, there are no reviews or comments for this patent.
If you have personal experience with Method of tellurium separation from copper electrorefining..., we encourage you to share that experience with our LandOfFree.com community. Your opinion is very important and Method of tellurium separation from copper electrorefining... will most certainly appreciate the feedback.
Profile ID: LFCA-PAI-O-1604221