ABSTRACT This invention is a method to prepare high strength high modulus polyolefin shaped articles comprising forming a heated solution of the polyolefin from particles of which about 75 to 100% by weight have a particle size of from about 100 to about 400 microns and having a weight average molecular weight of from about 300 000 to 7,000,000, then shaping the heated solution then cooling the shaped solution. To further increase the strength of the article it can be stretched.

516144

LandOfFree

Say what you really think

Search LandOfFree.com for Canadian inventors and patents. Rate them and share your experience with other people.

Rating

Method to prepare high strength ultrahigh molecular weight... does not yet have a rating. At this time, there are no reviews or comments for this patent.

If you have personal experience with Method to prepare high strength ultrahigh molecular weight..., we encourage you to share that experience with our LandOfFree.com community. Your opinion is very important and Method to prepare high strength ultrahigh molecular weight... will most certainly appreciate the feedback.

Rate now

     

Profile ID: LFCA-PAI-O-1285020

  Search
All data on this website is collected from public sources. Our data reflects the most accurate information available at the time of publication.