C09D 1/00 (2006.01) B05D 3/02 (2006.01) C23C 24/00 (2006.01)

Patent

CA 2711343

Methods for improving surface roughness of an environmental barrier coating (12) comprising: providing a component (10) having a plasma sprayed environmental barrier coating; applying a slurry to the environmental barrier coating of the component, the slurry comprising a transition layer slurry or an outer layer slurry; drying the environmental barrier coating having the applied slurry; and sintering the component to produce a component having an improved surface roughness wherein the slurry comprises: a solvent; a primary transition material, or a primary outer material; and a slurry sintering aid. aluminum salts, solvent soluble nickel salts, solvent titanium salts, solvent soluble boron salts, and solvent soluble alkaline earth salts.

LandOfFree

Say what you really think

Search LandOfFree.com for Canadian inventors and patents. Rate them and share your experience with other people.

Rating

Methods of improving surface roughness of an environmental... does not yet have a rating. At this time, there are no reviews or comments for this patent.

If you have personal experience with Methods of improving surface roughness of an environmental..., we encourage you to share that experience with our LandOfFree.com community. Your opinion is very important and Methods of improving surface roughness of an environmental... will most certainly appreciate the feedback.

Rate now

     

Profile ID: LFCA-PAI-O-2022891

  Search
All data on this website is collected from public sources. Our data reflects the most accurate information available at the time of publication.