A method of making scorodite includes the following steps: (1) an acidic aqueous solution containing pentavalent As and trivalent Fe is heated at a temperature for a time, the temperature and the time being effective for synthesis of crystalline scorodite; (2) the synthesized scorodite is separated from the post-reaction solution by solid-liquid separation; and (3) the scorodite is washed with water and is separated from the washing solution by solid-liquid separation. Step (3) is repeated until the concentration of at least one component of the post-reaction solution contained in the washing solution used for washing the scorodite decreases to a predetermined level.

LandOfFree

Say what you really think

Search LandOfFree.com for Canadian inventors and patents. Rate them and share your experience with other people.

Rating

Methods of making and washing scorodite does not yet have a rating. At this time, there are no reviews or comments for this patent.

If you have personal experience with Methods of making and washing scorodite, we encourage you to share that experience with our LandOfFree.com community. Your opinion is very important and Methods of making and washing scorodite will most certainly appreciate the feedback.

Rate now

     

Profile ID: LFCA-PAI-O-2049795

  Search
All data on this website is collected from public sources. Our data reflects the most accurate information available at the time of publication.