Mineral separation

B - Operations – Transporting – 03 – B

Patent

Rate now

  [ 0.00 ] – not rated yet Voters 0   Comments 0

Details

209/2

B03B 7/00 (2006.01) B03B 1/04 (2006.01) B03B 9/00 (2006.01) C22B 1/16 (2006.01) C22B 1/244 (2006.01) C22B 11/02 (2006.01) C22B 15/00 (2006.01)

Patent

CA 1218961

ABSTRACT Gold or any desired mineral treated to have a lyophilic surface, is recovered from ore bodies by an agglomeration method in which coal and oil are added to the ground or slurry and contacted in a zone where any agglomerates are kept below 500 microns in size. Subsequently the mix is passed to an agglomeration zone where agglomerates of coal oil and gold or the lyophilic mineral are formed. The agglomerates are separated from the gangue and recycled to the contacting zone until a desired gold or mineral concentration in the agglomer- ates is achieved.

452941

LandOfFree

Say what you really think

Search LandOfFree.com for Canadian inventors and patents. Rate them and share your experience with other people.

Rating

Mineral separation does not yet have a rating. At this time, there are no reviews or comments for this patent.

If you have personal experience with Mineral separation, we encourage you to share that experience with our LandOfFree.com community. Your opinion is very important and Mineral separation will most certainly appreciate the feedback.

Rate now

     

Profile ID: LFCA-PAI-O-1202117

  Search
All data on this website is collected from public sources. Our data reflects the most accurate information available at the time of publication.