ABSTRACT OF THE DISCLOSURE A minute acicular particle containing metallic iron, iron carbide and free carbon, which is produced by reducing iron carbide, has a mean particle diameter (major axis) of 0.1 - 0.5 µm and an average aspect ratio of 3 to 15, and contains 10-80 wt.% of metallic iron, 10-75 wt.% of iron carbide and 5-13 wt.% of free carbon.

LandOfFree

Say what you really think

Search LandOfFree.com for Canadian inventors and patents. Rate them and share your experience with other people.

Rating

Minute acicular particle containing metallic iron, iron... does not yet have a rating. At this time, there are no reviews or comments for this patent.

If you have personal experience with Minute acicular particle containing metallic iron, iron..., we encourage you to share that experience with our LandOfFree.com community. Your opinion is very important and Minute acicular particle containing metallic iron, iron... will most certainly appreciate the feedback.

Rate now

     

Profile ID: LFCA-PAI-O-1634295

  Search
All data on this website is collected from public sources. Our data reflects the most accurate information available at the time of publication.