ABSTRACT OF THE DISCLOSURE An Ni-base single-crystal superalloy consisting essentially of 9 - 11 % Cr; 0.5 - 0.8 % Mo; 5.5 - 6.8 % W; 5.2 - 6 % Ta; 5 - 6 % Al; 1.8 - 2.5 % Ti; 4.2 - 4.9 % Co; 0.05 - 0.5 % Re; and the balance of Ni and inevitable impurities. If required, the superalloy may further contain 0.01 - 0.3 % Si. The superalloy has a structure wherein a .gamma.'-phase formed of a fine intermetallic compound is dispersed evenly throughout the matrix, thereby being excellent in high- temperature strength as well as in high-temperature corrosion resistance.

610513

LandOfFree

Say what you really think

Search LandOfFree.com for Canadian inventors and patents. Rate them and share your experience with other people.

Rating

Ni-base single-crystal superalloy excellent in... does not yet have a rating. At this time, there are no reviews or comments for this patent.

If you have personal experience with Ni-base single-crystal superalloy excellent in..., we encourage you to share that experience with our LandOfFree.com community. Your opinion is very important and Ni-base single-crystal superalloy excellent in... will most certainly appreciate the feedback.

Rate now

     

Profile ID: LFCA-PAI-O-1204380

  Search
All data on this website is collected from public sources. Our data reflects the most accurate information available at the time of publication.