C22C 19/05 (2006.01) C22F 1/02 (2006.01) C22F 1/10 (2006.01) F01D 5/28 (2006.01) F01D 25/00 (2006.01) F02C 7/00 (2006.01) C22F 1/00 (2006.01)

Patent

CA 2749755

Disclosed is a Ni-based single crystal alloy which has a chemi-cal composition comprising 8 to 12% by mass of Co, 5 to 7.5% by mass of Cr, 0.2 to 1.2% by mass of Mo, 5 to 7% by mass of W, 5 to 6.5% by mass of Al, 8 to 12% by mass of Ta, 0.01 to 0.2% by mass of Hf, 2 to 4% by mass of Re and 0.005 to 0.1% by mass of Si, with the remainder being Ni and un--avoidable impurities, and is a single crystal.

L'invention concerne un alliage monocristallin à base de nickel dont la composition est la suivante : 8 à 12% en masse de Co, 5 à 7,5% en masse de Cr, 0,2 à 1,2% en masse de Mo, 5 à 7% en masse de W, 5 à 6,5% en masse de Al, 8 à 12% en masse de Ta, 0,01 à 0,2% en masse de Hf, 2 à 4% en masse de Re et 0,005 à 0.1% en masse de Si, la partie restante étant constituée de Ni et d'impuretés inévitables. L'alliage cristallin de l'invention est un monocristal.

LandOfFree

Say what you really think

Search LandOfFree.com for Canadian inventors and patents. Rate them and share your experience with other people.

Rating

Ni-based single crystal superalloy does not yet have a rating. At this time, there are no reviews or comments for this patent.

If you have personal experience with Ni-based single crystal superalloy, we encourage you to share that experience with our LandOfFree.com community. Your opinion is very important and Ni-based single crystal superalloy will most certainly appreciate the feedback.

Rate now

     

Profile ID: LFCA-PAI-O-1421555

  Search
All data on this website is collected from public sources. Our data reflects the most accurate information available at the time of publication.