An alloy having a combination of good corrosion resistance m sulfuric acid and resistance to localized attack in chloride-bearing, gas scrubbing systems has a composition in weight percent of 22.0% to 24.0% chromium, 15.0% to 16.5 % molybdenum, up to 1.5% iron, 0.14% to 0.46% copper, 0.1 % to 0.4% aluminum, up to 0.010% carbon, up to 0.3% cobalt, up to 0.5% manganese, up to 0.10% silicon, up to 0.015% phosphorus, up to 0.010% sulfur, and the balance nickel plus impurities.
Crook Paul
Dimock Stratton Llp
Haynes International Inc.
LandOfFree
Ni-cr-mo alloys having improved corrosion resistance does not yet have a rating. At this time, there are no reviews or comments for this patent.
If you have personal experience with Ni-cr-mo alloys having improved corrosion resistance, we encourage you to share that experience with our LandOfFree.com community. Your opinion is very important and Ni-cr-mo alloys having improved corrosion resistance will most certainly appreciate the feedback.
Profile ID: LFCA-PAI-O-1423636