ABSTRACT OF THE DISCLOSURE A member adapted for use under a stress in an atmosphere of a temperature below the creep temperature and made from an Ni base alloy having a high resistance to stress corrosion cracking. The Ni alloy consists essen- tially of, by weight, 15 to 25% of Cr, 1 to 8% of Mo, 0.4 to 2% of Al, 0.7 to 3% of Ti, 0.7 to 4.5% of Nb and the balance Ni, and has an austenite matrix in which precipitat- ed is at least on of Y' phase and Y" phase. The member can suitably used as parts which are subjected to pure water in nuclear reactor.

Application Number

393087

LandOfFree

Say what you really think

Search LandOfFree.com for Canadian inventors and patents. Rate them and share your experience with other people.

Rating

Nickel base alloy having high resistance to stress corrosion... does not yet have a rating. At this time, there are no reviews or comments for this patent.

If you have personal experience with Nickel base alloy having high resistance to stress corrosion..., we encourage you to share that experience with our LandOfFree.com community. Your opinion is very important and Nickel base alloy having high resistance to stress corrosion... will most certainly appreciate the feedback.

Rate now

     

Profile ID: LFCA-PAI-O-1242719

  Search
All data on this website is collected from public sources. Our data reflects the most accurate information available at the time of publication.