ABSTRACT OF THE DISCLOSURE A nickel-base superalloy cast article is provided with improved stress rupture and creep properties as a result of providing its microstructure with aligned cellular dendrites in combination with the substantial absence of NiAl, carbon, carbides, and Ti. The superalloy consists, in atomic percent, essentially of 4-11 Cr. 5-16 Al, at least 0.5 R?, up to about 10V, up to about 15 Co, up to about 5 Ta, up to about 5W, up to about 1 Mo, up to about 2.5 Mn, up to about 2.5 Rh, with the balance nickel and incidental impurities. The alloy is suited for use in gas turbines.

215680

LandOfFree

Say what you really think

Search LandOfFree.com for Canadian inventors and patents. Rate them and share your experience with other people.

Rating

Nickel-base superalloy cast article does not yet have a rating. At this time, there are no reviews or comments for this patent.

If you have personal experience with Nickel-base superalloy cast article, we encourage you to share that experience with our LandOfFree.com community. Your opinion is very important and Nickel-base superalloy cast article will most certainly appreciate the feedback.

Rate now

     

Profile ID: LFCA-PAI-O-521883

  Search
All data on this website is collected from public sources. Our data reflects the most accurate information available at the time of publication.