Nickel-base superalloys and components formed thereof

C - Chemistry – Metallurgy – 22 – C

Patent

Rate now

  [ 0.00 ] – not rated yet Voters 0   Comments 0

Details

C22C 19/05 (2006.01) B23P 15/02 (2006.01) C22C 1/04 (2006.01) C22C 30/00 (2006.01)

Patent

CA 2704874

A gamma prime nickel-base superalloy and components formed therefrom that exhibit improved high-temperature dwell capabilities, including creep and hold time fatigue crack growth behavior. A particular example of a component is a powder metallurgy turbine disk of a gas turbine engine. The gamma-prime nickel-base superalloy contains, by weight, 16.0 to 30.0% cobalt, 11.5 to 15.0% chromium, 4.0 to 6.0% tantalum, 2.0 to 4.0% aluminum, 1.5 to 6.0% titanium, up to 5.0% tungsten, 1.0 to 7.0% molybdenum, up to 3.5% niobium, up to 1.0% hafnium, 0.02 to 0.20% carbon, 0.01 to 0.05% boron, 0.02 to 0.10% zirconium, the balance essentially nickel and impurities, wherein the titanium: aluminum weight ratio is 0.5 to 2Ø

LandOfFree

Say what you really think

Search LandOfFree.com for Canadian inventors and patents. Rate them and share your experience with other people.

Rating

Nickel-base superalloys and components formed thereof does not yet have a rating. At this time, there are no reviews or comments for this patent.

If you have personal experience with Nickel-base superalloys and components formed thereof, we encourage you to share that experience with our LandOfFree.com community. Your opinion is very important and Nickel-base superalloys and components formed thereof will most certainly appreciate the feedback.

Rate now

     

Profile ID: LFCA-PAI-O-1480817

  Search
All data on this website is collected from public sources. Our data reflects the most accurate information available at the time of publication.