The superalloy according to the invention, suitable for the manufacture of turbo-engine parts by monocrystallization solidification, possesses the following mass composition: Cr : 3.5 to 7.5 % Mo : 0 to 1.5 % Re : 1.5 to 5.5 % Ru : 0 to 5.5 % W : 3.5 to 8.5 % Al : 5 to 6.5 % Ti : 0 to 2.5 % Ta : 4.5 to 9 % Hf : 0.08 to 0.12 % Si : 0.08 to 0.12 % the complement to 100 % consisting of Ni and possible impurities.
Caron Pierre
Naveos Serge
Raffestin Jean-Louis
Norton Rose Or S.e.n.c.r.l. S.r.l./llp
Onera (office National D'etudes Et de Recherches Aerospatiales)
LandOfFree
Nickel-based monocrystalline superalloy with a high .gamma.'... does not yet have a rating. At this time, there are no reviews or comments for this patent.
If you have personal experience with Nickel-based monocrystalline superalloy with a high .gamma.'..., we encourage you to share that experience with our LandOfFree.com community. Your opinion is very important and Nickel-based monocrystalline superalloy with a high .gamma.'... will most certainly appreciate the feedback.
Profile ID: LFCA-PAI-O-1971153