A protective coating system for superalloys is described. The coating is an yttrium enriched aluminide, and can be formed by aluminizing an MCrAlY or overlay coated superalloy, wherein during the aluminizing process, aluminum diffuses completely through the MCrAlY coating and into the substrate. The coating system exhibits desirable oxidation resistance and resistance to thermal fatigue cracking.
Gupta Dinesh K.
Olson Walter E.
Gupta Dinesh K.
Ogilvy Renault Llp/s.e.n.c.r.l.,s.r.l.
Olson Walter E.
United Technologies Corporation
LandOfFree
Nickel or cobalt base superalloy article having an aluminide... does not yet have a rating. At this time, there are no reviews or comments for this patent.
If you have personal experience with Nickel or cobalt base superalloy article having an aluminide..., we encourage you to share that experience with our LandOfFree.com community. Your opinion is very important and Nickel or cobalt base superalloy article having an aluminide... will most certainly appreciate the feedback.
Profile ID: LFCA-PAI-O-1680575