FN: 4363h. CAN lA OIL TREATED MINERAL FILLER FOR ASPHALT Abstract of the Disclosure Use of surface modification treatment on mineral fines to obtain higher filler loadings in asphalt used for roofing shingles. Mineral fines are coated with oil such as a petroleum oil at about the 0.25 - 1.0 percent level before they are incorporated into molten asphalt. This treatment makes minerals which otherwise would be uncompetitive with traditional fillers, such as limestone, sufficiently compatible with asphalt to be a viable alternative to limestone. Nepheline syenite mineral fines treated in this manner have been successfully incorporated into asphalt for shingles at a loading of 65 - 70%.

LandOfFree

Say what you really think

Search LandOfFree.com for Canadian inventors and patents. Rate them and share your experience with other people.

Rating

Oil treated mineral filler for asphalt does not yet have a rating. At this time, there are no reviews or comments for this patent.

If you have personal experience with Oil treated mineral filler for asphalt, we encourage you to share that experience with our LandOfFree.com community. Your opinion is very important and Oil treated mineral filler for asphalt will most certainly appreciate the feedback.

Rate now

     

Profile ID: LFCA-PAI-O-1389066

  Search
All data on this website is collected from public sources. Our data reflects the most accurate information available at the time of publication.