Optimizing the yield of maleic anhydride catalyst

C - Chemistry – Metallurgy – 07 – D

Patent

Rate now

  [ 0.00 ] – not rated yet Voters 0   Comments 0

Details

260/365.7

C07D 307/60 (2006.01) B01J 27/198 (2006.01) C07C 51/215 (2006.01)

Patent

CA 1259622

Optimizing the Yield of Maleic Anhydride Catalyst Inventors Mitchell Becker John Walden Abstract A method of optimizing the yield of a vanadium-phosphorus catalyst during the oxidation of butane to maleic anhydride, which comprises establishing the temperature at which the catalyst provides the desired percentage conversion and yield of maleic anhydride with the established feed composition and then maintaining that temperature by continuously introducing an amount of a suitable phosphorus compound necessary to pre- vent a decline in selectivity to maleic anhydride without significantly increasing the temperature. 1275

489931

LandOfFree

Say what you really think

Search LandOfFree.com for Canadian inventors and patents. Rate them and share your experience with other people.

Rating

Optimizing the yield of maleic anhydride catalyst does not yet have a rating. At this time, there are no reviews or comments for this patent.

If you have personal experience with Optimizing the yield of maleic anhydride catalyst, we encourage you to share that experience with our LandOfFree.com community. Your opinion is very important and Optimizing the yield of maleic anhydride catalyst will most certainly appreciate the feedback.

Rate now

     

Profile ID: LFCA-PAI-O-1167402

  Search
All data on this website is collected from public sources. Our data reflects the most accurate information available at the time of publication.