Polyurethane elastomers exhibiting improved green strength while maintaining short demold times are prepared from ultra-low unsaturation polyoxypropylene polyols containing up to 20 weight percent internal random oxyethylene moieties. The elastomers adsorb less than 10 weight percent water at 0°C. The internal polyoxyethylene moiety-containing polyoxypropylene polyols may be used to prepare ultra-low unsaturation polyoxyethylene capped polyols which are haze-free and which may be used to prepare haze-free 4,4'-MDI prepoly-mers. Multidisperse blends of monodisperse internal oxyethylene moiety-containing polyoxypropylene polyols of ultra-low unsaturation provide yet further improve-ments in elastomer processing.
Allen Gary L.
Barksby Nigel
Isaacs Bruce H.
Langsdorf Leah J.
Seneker Stephen D.
Arco Chemical Technology L.p.
Bayer Antwerp N.v.
Norton Rose Or S.e.n.c.r.l. S.r.l./llp
LandOfFree
Polyurethane elastomers exhibiting improved demold, green... does not yet have a rating. At this time, there are no reviews or comments for this patent.
If you have personal experience with Polyurethane elastomers exhibiting improved demold, green..., we encourage you to share that experience with our LandOfFree.com community. Your opinion is very important and Polyurethane elastomers exhibiting improved demold, green... will most certainly appreciate the feedback.
Profile ID: LFCA-PAI-O-1467531