Pre-hip heat treatment of superalloy castings

B - Operations – Transporting – 22 – F

Patent

Rate now

  [ 0.00 ] – not rated yet Voters 0   Comments 0

Details

75/165

B22F 3/12 (2006.01) C21D 8/00 (2006.01) C22F 1/10 (2006.01)

Patent

CA 1243508

-12- Pre-Hip Heat Treatment of Superalloy Castings Abstract Heat treatments are described which improve subsequent HIP treatment results of superalloy articles. The heat treatments substantially eliminate certain low melting phases which other- wise would cause problems relating to gas entrap- ment during a HIP process. The articles are heated to a temperature near but below the intended HIP temperature for a period of time sufficient to reduce the low melting phase.

468428

LandOfFree

Say what you really think

Search LandOfFree.com for Canadian inventors and patents. Rate them and share your experience with other people.

Rating

Pre-hip heat treatment of superalloy castings does not yet have a rating. At this time, there are no reviews or comments for this patent.

If you have personal experience with Pre-hip heat treatment of superalloy castings, we encourage you to share that experience with our LandOfFree.com community. Your opinion is very important and Pre-hip heat treatment of superalloy castings will most certainly appreciate the feedback.

Rate now

     

Profile ID: LFCA-PAI-O-1173092

  Search
All data on this website is collected from public sources. Our data reflects the most accurate information available at the time of publication.