A precipitation-hardenable nickel-base superalloy with improved mechanical properties in the temperature range from 600 to 750°C which has the following composition: Cr = 12 - 15 per cent by weight Co = 3 - 4.5 per cent by weight W = 1 - 3.5 per cent by weight Ta = 4 - 5.5 per cent by weight Al = 3 - 4.3 per cent by weight Ti = 4 - 5 per cent by weight Hf = 0 - 2.5 per cent by weight B = 0 -0.02 per cent by weight Zr = 0.01-0.06 per cent by weight C = 0.05-0.07 per cent by weight Ni = remainder.

592074

LandOfFree

Say what you really think

Search LandOfFree.com for Canadian inventors and patents. Rate them and share your experience with other people.

Rating

Precipitation-hardenable nickel-base superalloy with... does not yet have a rating. At this time, there are no reviews or comments for this patent.

If you have personal experience with Precipitation-hardenable nickel-base superalloy with..., we encourage you to share that experience with our LandOfFree.com community. Your opinion is very important and Precipitation-hardenable nickel-base superalloy with... will most certainly appreciate the feedback.

Rate now

     

Profile ID: LFCA-PAI-O-1195928

  Search
All data on this website is collected from public sources. Our data reflects the most accurate information available at the time of publication.