Preparation of binderless 3a adsorbents

B - Operations – Transporting – 01 – J

Patent

Rate now

  [ 0.00 ] – not rated yet Voters 0   Comments 0

Details

182/10, 252/33

B01J 29/06 (2006.01) B01D 15/04 (2006.01) B01J 20/18 (2006.01) C07C 7/13 (2006.01)

Patent

CA 1181387

Abstract of the Disclosure Shaped products of a 3A zeolite are formed either as beads or extrudates without any binder remaining. In the case of beads, a 4A powder is mixed with a caustic solution and a metakaolin clay binder to form beads. The beads are converted to a binderless 4A product which is given a partial calcium exchange followed by a potassium exchange to obtain the desired 3A binderless bead. The 3A extrudates are produced by forming binderless 4A extrudates from a 4A powder and clay mixture that contains 40-60% by weight clay. These binderless 4A extrudates are then given a potassium exchange. Both the beads and the extrudates can be used to dry a mixture of a hydrocarbon compound such as ethylene and water.

411628

LandOfFree

Say what you really think

Search LandOfFree.com for Canadian inventors and patents. Rate them and share your experience with other people.

Rating

Preparation of binderless 3a adsorbents does not yet have a rating. At this time, there are no reviews or comments for this patent.

If you have personal experience with Preparation of binderless 3a adsorbents, we encourage you to share that experience with our LandOfFree.com community. Your opinion is very important and Preparation of binderless 3a adsorbents will most certainly appreciate the feedback.

Rate now

     

Profile ID: LFCA-PAI-O-1187326

  Search
All data on this website is collected from public sources. Our data reflects the most accurate information available at the time of publication.