CA 1328981
IMPROVEMENTS IN THE PREPARATION OF COPPER ARSENATE ABSTRACT Copper arsenate, substantially free from impurities that will form a sludge in the process for producing wood preservatives such as chromated copper arsenate and having a water content of less than 15%, is prepared by mixing a solution of soluble arsenate and a copper sulfate solution, either or both solutions containing sludge-forming impurities, to form a copper and arsenic-containing solution without precipitating copper arsenate. The pH during the adding is controlled at a value in the range of 1.7 to 2.2 to precipitate impurities. Precipitated impurities are removed, and the copper and arsenic-containing solution is neutralized with a suitable alkaline substance, preferably dilute sodium hydroxide solution, to pH 3.2 to 4.2 to precipitate copper arsenate. The water content of the copper arsenate is reduced by adding to the copper and arsenic-containing solution, either in the mixing of arsenate solution with copper sulfate solution or in the precipitation of copper arsenate, an amount of soluble chromium in the range of about 0.005 to 0.250 gram chromium per litre of solution.
609402
Knoerr Susan B.
Robins Robert G.
Gowling Lafleur Henderson Llp
Teck Cominco Metals Ltd.
LandOfFree
Preparation of copper arsenate does not yet have a rating. At this time, there are no reviews or comments for this patent.
If you have personal experience with Preparation of copper arsenate, we encourage you to share that experience with our LandOfFree.com community. Your opinion is very important and Preparation of copper arsenate will most certainly appreciate the feedback.
Profile ID: LFCA-PAI-O-1182437