Preparation of low molecular weight cellulose esters

C - Chemistry – Metallurgy – 08 – B

Patent

Rate now

  [ 0.00 ] – not rated yet Voters 0   Comments 0

Details

C08B 3/00 (2006.01) C08B 3/02 (2006.01) C08B 3/06 (2006.01) C08B 3/24 (2006.01)

Patent

CA 2078876

2078876 9116356 PCTABS00007 A process is disclosed for the preparation of low molecular weight, high hydroxyl cellulose esters ideally suited for use in coating applications. The new synthetic procedure involves treating a cellulose polymer with trifluoroacetic acid, a mineral acid, an acyl or aryl anhydride in an appropriate carboxylic solvent followed by, optionally, in situ hydrolysis. Typical reaction times for conversion to a triester are 5 to 30 minutes while typical hydrolysis times for far hydrolyzed mixed esters range from 4 to 7 hours. Molecular weight loss occurs during formation of the cellulose triester permitting concentrated reaction mixtures and easier isolation of the product ester.

LandOfFree

Say what you really think

Search LandOfFree.com for Canadian inventors and patents. Rate them and share your experience with other people.

Rating

Preparation of low molecular weight cellulose esters does not yet have a rating. At this time, there are no reviews or comments for this patent.

If you have personal experience with Preparation of low molecular weight cellulose esters, we encourage you to share that experience with our LandOfFree.com community. Your opinion is very important and Preparation of low molecular weight cellulose esters will most certainly appreciate the feedback.

Rate now

     

Profile ID: LFCA-PAI-O-1945151

  Search
All data on this website is collected from public sources. Our data reflects the most accurate information available at the time of publication.