Preparation of triethyl dimethyl siloxalane

C - Chemistry – Metallurgy – 07 – F

Patent

Rate now

  [ 0.00 ] – not rated yet Voters 0   Comments 0

Details

260/432.3

C07F 7/08 (2006.01) C08F 10/00 (2006.01)

Patent

CA 1227807

ABSTRACT OF THE DISCLOSURE A process for the preparation of triethyl dimethyl siloxalane is disclosed. The process comprises admixing octamethylcyclotetrasiloxane with triethyl aluminum, optionally in the presence of an inert hydrocarbon solvent, at a temperature of 170-250°C for a period of at least 10 minutes. The molar ratio of triethyl aluminum to octamethylcyclotetrasiloxane is at least 3.9:1 and preferably 3.9-4.5:1. The siloxalane may be used as a co-catalyst in the polymerization of ethylene and/or other alpha-olefins.

458020

LandOfFree

Say what you really think

Search LandOfFree.com for Canadian inventors and patents. Rate them and share your experience with other people.

Rating

Preparation of triethyl dimethyl siloxalane does not yet have a rating. At this time, there are no reviews or comments for this patent.

If you have personal experience with Preparation of triethyl dimethyl siloxalane, we encourage you to share that experience with our LandOfFree.com community. Your opinion is very important and Preparation of triethyl dimethyl siloxalane will most certainly appreciate the feedback.

Rate now

     

Profile ID: LFCA-PAI-O-1283708

  Search