Patent

CA 1054871

ABSTRACT OF THE DISCLOSURE The adhesive strength of a metallic layer prepared by vacuum metallizing on an unsaturated carboxylic acid modified polyolefin article is substantially increased by heating below the melting point of the polyolefin after the metallization. Preferable heating temperature is 92 - 157°C for polypropylene and heating time is 10 sec. - 1 hour. An aluminum layer obtained by this invention has remaining ratio of 100% after cross cut test.

226637

LandOfFree

Say what you really think

Search LandOfFree.com for Canadian inventors and patents. Rate them and share your experience with other people.

Rating

Process and product does not yet have a rating. At this time, there are no reviews or comments for this patent.

If you have personal experience with Process and product, we encourage you to share that experience with our LandOfFree.com community. Your opinion is very important and Process and product will most certainly appreciate the feedback.

Rate now

     

Profile ID: LFCA-PAI-O-1010262

  Search
All data on this website is collected from public sources. Our data reflects the most accurate information available at the time of publication.