Process for a selective flotation of a copper-lead-zinc sulfide

B - Operations – Transporting – 03 – D

Patent

Rate now

  [ 0.00 ] – not rated yet Voters 0   Comments 0

Details

B03D 1/02 (2006.01) B03B 1/00 (2006.01) B03D 1/06 (2006.01)

Patent

CA 2107275

-18- ABSTRACT PROCESS FOR A SELECTIVE FLOTATION OF COPPER-LEAD- ZINC SULFIDE ORES In a process for a selective flotation of a copper-lead-zinc sulfide ore the raw ore is ground and slurried with water and the resulting suspension is aerated with air to adjust a certain oxidation-reduction potential and is subsequently successively conditioned with SO2, Ca(OH)2, and collecting and frothing agents, whereafter a flota- tion of Cu is effected. An oxidation-reduction poten- tial which is 70 to 90% of the oxidation-reduction potential desired for the flotation of Cu is adjusted by the aeration of the suspension with air before the flotation of Cu, the desired oxidation-reduction po- tential of 60 to 340 mV is adjusted during the flota- tion of Cu by the aeration with air, the flotation of Cu is effected at a pH of 8.5 to 10.5 and Cu is removed from the flotation process with the froth.

LandOfFree

Say what you really think

Search LandOfFree.com for Canadian inventors and patents. Rate them and share your experience with other people.

Rating

Process for a selective flotation of a copper-lead-zinc sulfide does not yet have a rating. At this time, there are no reviews or comments for this patent.

If you have personal experience with Process for a selective flotation of a copper-lead-zinc sulfide, we encourage you to share that experience with our LandOfFree.com community. Your opinion is very important and Process for a selective flotation of a copper-lead-zinc sulfide will most certainly appreciate the feedback.