ABSTRACT In a process according to the present invention pre-reduced lateritic ores containing iron and nickel are leached with an aqueous sulphuric acid leach liquor containing or into which is introduced in the presence of the ore a peroxidant selected from hydrogen peroxide and peroxymonosulphuric acid. By so doing, the liquor is obtained with a lower concentration of iron than if the peroxidant had not been employed. In preferred embodiments the leaching is carried out at from 40 to 70°C for a period of I to 5 hours; when hydrogen peroxide is used, it is preferably introduced continuously or progressively throughout the reaction period and when peroxymonosulphuric acid is used it is preferably introduced initially. The acidity of the liquor can be reduced at the end of the reaction to pH3 to 4 to further lower the content of iron in solution.
299226
Burkin Alfred R.
Monhemius Andrew J.
George H. Riches And Associates
Interox Chemicals Limited
LandOfFree
Process for extracting nickel from pre-reduced lateritic ore does not yet have a rating. At this time, there are no reviews or comments for this patent.
If you have personal experience with Process for extracting nickel from pre-reduced lateritic ore, we encourage you to share that experience with our LandOfFree.com community. Your opinion is very important and Process for extracting nickel from pre-reduced lateritic ore will most certainly appreciate the feedback.
Profile ID: LFCA-PAI-O-445944