18/800

B29C 47/38 (2006.01) B29C 47/00 (2006.01) C08G 18/40 (2006.01) C08G 18/42 (2006.01) C08G 63/91 (2006.01)

Patent

CA 1175623

ABSTRACT Poly(ethylene terephthalate) resin and blends of poly(ethylene terephthalate) resin with other polymers are extruded while being coupled with an organic diisocyanate under conditions where carbon dioxide gas is vented smoothly, as it is formed. The extruder has a number of zones designed to perform specific functions. The temperature in the kneading zone and in the venting zone must be maintained at about 280-320°C to bring about rapid reaction and to permit efficient gas evolution and removal without thermally degrading the polymeric material. The extruded article is free of trapped gas bubbles and other imperfections. This process is particularly suitable for making PET billets, which then are stretched to form strapping useful in packaging applications.

393931

LandOfFree

Say what you really think

Search LandOfFree.com for Canadian inventors and patents. Rate them and share your experience with other people.

Rating

Process for extruding a modified high molecular weight... does not yet have a rating. At this time, there are no reviews or comments for this patent.

If you have personal experience with Process for extruding a modified high molecular weight..., we encourage you to share that experience with our LandOfFree.com community. Your opinion is very important and Process for extruding a modified high molecular weight... will most certainly appreciate the feedback.

Rate now

     

Profile ID: LFCA-PAI-O-1209624

  Search
All data on this website is collected from public sources. Our data reflects the most accurate information available at the time of publication.