PROCESS FOR FABRICATING HIGH STRENGTH ALUMINUM SHEET ABSTRACT OF THE INVENTION The yield strength of aluminum sheet is increased by work hardening the aluminum at a temperature in the range of 150°-400°F. * * * * * * *