ABSTRACT OF THE DISCLOSURE The direct hydrothermal production of high purity sodium silicate solutions having a high SiO2 : Na2O molar ratio by reaction of a silicon dioxide source with aqueous sodium hydroxide solutions, or with aqueous sodium silicate solutions having a lower SiO2 : Na2O molar ratio, is made possible by using a silicon dioxide source that contains a sufficient fraction of cristobalite phase, or by condition- ing other crystalline forms of silicon dioxide by heating at or above 1100° C, but below the melting point of silica, before the hydrothermal treatment. Preferably the sodium hydroxide solution has a concentration range of 10 to 50% by weight, and the reaction is carried out in a closed pressure reactor at temperatures of 150 to 300°C and under saturated steam pressures corresponding to those tempera- tures.
Hoff Alfred
Novotny Rudolf
Schuertz Jost
Borden Ladner Gervais Llp
Henkel Kommanditgesellschaft Auf Aktien
LandOfFree
Process for hydrothermal production of sodium silicate... does not yet have a rating. At this time, there are no reviews or comments for this patent.
If you have personal experience with Process for hydrothermal production of sodium silicate..., we encourage you to share that experience with our LandOfFree.com community. Your opinion is very important and Process for hydrothermal production of sodium silicate... will most certainly appreciate the feedback.
Profile ID: LFCA-PAI-O-1833307