Process for in-situ leaching of uranium

E - Fixed Constructions – 21 – B

Patent

Rate now

  [ 0.00 ] – not rated yet Voters 0   Comments 0

Details

166/30

E21B 43/28 (2006.01) C22B 60/02 (2006.01)

Patent

CA 1117003

9960 Abstract Process for the in-situ leaching of uranium from a subterranean ore deposit employing a lixiviant containing a carbonate leaching agent and an oxidizing agent. The lixiviant is heated to a temperature of at least 110° F. prior to injection into the subterranean ore deposit. The use of a heated lixiviant provides for a substantially greater ultimate uranium recovery than that attained through the use of a lixiviant injected at ambient temperature conditions. The process may be carried out in several stages. In the first stage, a relatively low temperature lixiviant is injected. This is followed by a second stage in which the lixiviant is heated to an elevated temperature and then injected into the deposit. The invention is particularly applicable for use in subterranean deposits which contain uranium associated with carbonaceous material.

336020

LandOfFree

Say what you really think

Search LandOfFree.com for Canadian inventors and patents. Rate them and share your experience with other people.

Rating

Process for in-situ leaching of uranium does not yet have a rating. At this time, there are no reviews or comments for this patent.

If you have personal experience with Process for in-situ leaching of uranium, we encourage you to share that experience with our LandOfFree.com community. Your opinion is very important and Process for in-situ leaching of uranium will most certainly appreciate the feedback.

Rate now

     

Profile ID: LFCA-PAI-O-439850

  Search
All data on this website is collected from public sources. Our data reflects the most accurate information available at the time of publication.