Process for increasing the water solubility of gypsum

C - Chemistry – Metallurgy – 04 – B

Patent

Rate now

  [ 0.00 ] – not rated yet Voters 0   Comments 0

Details

C04B 11/024 (2006.01) C01F 11/46 (2006.01) C05D 3/00 (2006.01)

Patent

CA 2294987

A process for increasing the water solubility of gypsum in which gypsum is ground to about 5 to 20 mesh U.S. Standard Sieve Size, about 5 to 95 parts by weight of ground gypsum are mixed with about 2 to 25 parts by weight concentrated sulfuric acid having a concentration of about 93 to 98.5% H2SO4, optionally in the presence of about 5 to 20 parts by weight water, and the resulting products is dried at a temperature of about 100-125° C. to form a water soluble, granular, solid, free-flowing gypsum product having a water solubility increased by about 2- to greater than 350-fold.

LandOfFree

Say what you really think

Search LandOfFree.com for Canadian inventors and patents. Rate them and share your experience with other people.

Rating

Process for increasing the water solubility of gypsum does not yet have a rating. At this time, there are no reviews or comments for this patent.

If you have personal experience with Process for increasing the water solubility of gypsum, we encourage you to share that experience with our LandOfFree.com community. Your opinion is very important and Process for increasing the water solubility of gypsum will most certainly appreciate the feedback.

Rate now

     

Profile ID: LFCA-PAI-O-1407251

  Search
All data on this website is collected from public sources. Our data reflects the most accurate information available at the time of publication.