ABSTRACT OF THE DISCLOSURE In making a lead electrode for a lead-acid accumulator or the like, a supporting body of titanium is pickled in a boiling solution of oxalic acid and then adsorptively coated with a titanium (IV) layer in a treatment bath. This treatment is followed by the anodic coating of the titanium body with PbO2 in an electrolyte containing the lens of lead (II), in the presence of a lead (II) nitrate or a lead (II) salt of an amido. imido, nitride or fluoro sulfate or phosphate. The treatment bath may be an aqueous solution of an organic titanium salt, the pickling solution, or the electrolyte. If the pickling solution is used for this purpose, the titanium body is anodically connected or the solution is oxygenated. If the electrolyte is utilized, Ti(IV) ions are introduced into that liquid in which the titanium body is immersed for an extended period before closure of the anodizing circuit.

235633

LandOfFree

Say what you really think

Search LandOfFree.com for Canadian inventors and patents. Rate them and share your experience with other people.

Rating

Process for making titanium supported lead electrode does not yet have a rating. At this time, there are no reviews or comments for this patent.

If you have personal experience with Process for making titanium supported lead electrode, we encourage you to share that experience with our LandOfFree.com community. Your opinion is very important and Process for making titanium supported lead electrode will most certainly appreciate the feedback.

Rate now

     

Profile ID: LFCA-PAI-O-511950

  Search
All data on this website is collected from public sources. Our data reflects the most accurate information available at the time of publication.