Process for manufacturing chemo-mechanical and/or...

D - Textiles – Paper – 21 – C

Patent

Rate now

  [ 0.00 ] – not rated yet Voters 0   Comments 0

Details

D21C 1/04 (2006.01) D21B 1/16 (2006.01) D21C 3/20 (2006.01)

Patent

CA 2067129

2067129 9105102 PCTABS00004 In a process for manufacturing chemo-mechanical and/or chemo-thermo-mechanical wood pulps, raw materials containing lignocellulose, such as wood shavings, wood chips, pre-ground wood or sawdust, are first impregnated with an aqueous alcoholic SO2 solution and then heated to a temperature between 50 and 170 ·C for a period of 1 to 300 minutes. The wood shavings are then ground to the desired degree of fineness in a defibrinating device which is known per se. The process makes it possible to achieve up to 50 % reduction in grinding energy in comparison with known chemo-thermo-mechanical processes.

LandOfFree

Say what you really think

Search LandOfFree.com for Canadian inventors and patents. Rate them and share your experience with other people.

Rating

Process for manufacturing chemo-mechanical and/or... does not yet have a rating. At this time, there are no reviews or comments for this patent.

If you have personal experience with Process for manufacturing chemo-mechanical and/or..., we encourage you to share that experience with our LandOfFree.com community. Your opinion is very important and Process for manufacturing chemo-mechanical and/or... will most certainly appreciate the feedback.

Rate now

     

Profile ID: LFCA-PAI-O-2075652

  Search
All data on this website is collected from public sources. Our data reflects the most accurate information available at the time of publication.