A hydrophobic zeolite is prepared having high Hydrophobicity Index number by calcining a zeolite with steam under turbulent condition with respect to flow pattern of the zeolite and at a temperature within the range of 650-1000 °C.
La présente invention concerne la préparation d'une zéolithe hydrophobe, ayant un indice d'hydrophobicité élevé, par calcination d'une zéolithe au moyen de vapeur, dans des conditions de turbulence qui prennent en considération la courbe d'écoulement de la zéolithe et dont la température oscille entre 650-1000 DEG C.
Cooper David A.
Cormier William E.
Hertzenberg Elliot P.
Hinchey Richard J.
Marcus Bonita K.
Goudreau Gage Dubuc
Pq Holding Inc.
LandOfFree
Process for preparing a modified zeolite does not yet have a rating. At this time, there are no reviews or comments for this patent.
If you have personal experience with Process for preparing a modified zeolite, we encourage you to share that experience with our LandOfFree.com community. Your opinion is very important and Process for preparing a modified zeolite will most certainly appreciate the feedback.
Profile ID: LFCA-PAI-O-1456753