The present invention provides a process for preparing a raw material powder for producing a sintered body of aluminum titanate comprising: pulverizing a mixture containing: (1) 100 parts by weight of aluminum titanate crystals pulverized until a maximum grain size of 30 to 50 µm is attained; and (2) 2 to 6 parts by weight of spinel crystals obtained by heating a mixture containing MgO and Al2O3 at 1250°C to 1290°, a molar ratio of MgO to Al2Og being 1:0.95 to 1:1.05, said pulverizing being conducted by wet grinding process with a ball mill or cylinder mill.

LandOfFree

Say what you really think

Search LandOfFree.com for Canadian inventors and patents. Rate them and share your experience with other people.

Rating

Process for preparing sintered body of aluminum titanate does not yet have a rating. At this time, there are no reviews or comments for this patent.

If you have personal experience with Process for preparing sintered body of aluminum titanate, we encourage you to share that experience with our LandOfFree.com community. Your opinion is very important and Process for preparing sintered body of aluminum titanate will most certainly appreciate the feedback.

Rate now

     

Profile ID: LFCA-PAI-O-1717431

  Search
All data on this website is collected from public sources. Our data reflects the most accurate information available at the time of publication.