A B S T R A C T "PROCESS FOR PRODUCING A SMOOTH POLYESTER YARN AND POLYESTER YARN PRODUCED BY SAID PROCESS" In a process for producing a smoothy, low-shrinkage polyester filament yarn, the starting point is high-speed spun POY. The polyester POY is cold-drawn and then subjected to a hot relaxation under an overfeed of 10 to 20% at 140 to 250°C in a dry medium or at 70 to 140°C in a wet medium and if desired intermingled. The result is a yarn having an initial modulus of 200 to 800 cN/tex and a boil shrinkage of less than 3%. The yarn is suitable for use as a replacement material for cellulose acetate.

549570

LandOfFree

Say what you really think

Search LandOfFree.com for Canadian inventors and patents. Rate them and share your experience with other people.

Rating

Process for producing a smooth polyester yarn and polyester... does not yet have a rating. At this time, there are no reviews or comments for this patent.

If you have personal experience with Process for producing a smooth polyester yarn and polyester..., we encourage you to share that experience with our LandOfFree.com community. Your opinion is very important and Process for producing a smooth polyester yarn and polyester... will most certainly appreciate the feedback.

Rate now

     

Profile ID: LFCA-PAI-O-1314720

  Search
All data on this website is collected from public sources. Our data reflects the most accurate information available at the time of publication.